Al-Sc 20μm-63μm

Aluminum-Scandium (Al-Sc) alloy powder, with a particle size range of 20-63 µm, is engineered for advanced manufacturing, offering a unique combination of high strength, excellent weldability, and improved corrosion resistance. This advanced alloy benefits from the addition of scandium, enhancing grain refinement and elevating mechanical properties, making it highly suitable for aerospace and automotive applications. Al-Sc's superior performance at high temperatures and its ability to undergo heat treatment make it a prime choice for components requiring strength and durability under extreme conditions.

The 20-63 µm particle size suggests good spreadability for recoating systems with recoat speeds up to 170 mm/s, essential for producing parts with intricate designs and high-quality finishes. Other tailored particle size distributions are available upon request.

Powder designed for

Directed Energy Deposition

Powder Bed Fusion

Al-Sc

MPW metal powder is manufactured utilizing our DirectPowder™ process. The mechanical only, high-yield, no-melt technology maintains the microstructure and temper of the bar stock material, yielding a consistent size and shape and narrow particle size distribution.

Technical Data

  • Element Weight %

    Al bal.

    Mg 4.2% - 5.1%

    Sc 0.6% - 0.88%

    Mn 0.3% - 0.8%

    Zr 0.2% - 0.5%

    Fe ≤ 0.4%

    Si ≤ 0.4%

    Zn ≤ 0.25%

    Ti ≤ 0.15%

    Cu ≤ 0.1%

    V ≤ 0.1%

    O ≤ 0.05%

  • Nominal particle size: 20-63 μm. Other tailored PSDs available upon request.

  • Laser Diffraction: ASTM B822/ISO13320, Results Pending

    Apparent Density: ASTM B329, 1.0 g/cm3

    Tap Density: ASTM B527, 1.4 g/cm3

  • Material shall be packaged in UN certified 1L or 4L HDPE containers. Containers shall be marked with the following: Material Designation, Batch Number, Particle Size, Quantity (kg), and Customer PO Number.